301-10 Specifications for Structural Concrete Topic: Specifications Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 301 Published: 12/2010 Regular Price: $ 101.50 USD Member Price: $ 63.00 USD Become a Member More Info »
301-05: Specifications for Structural Concrete Topic: Specifications Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 301 Published: 8/2005 Regular Price: $ 87.50 USD Member Price: $ 50.00 USD Become a Member More Info »
233R-03: Slag Cement in Concrete and Mortar (Reapproved 2011) Topic: Slag Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 233 Published: 9/2003 Regular Price: $ 61.50 USD Member Price: $ 38.00 USD Become a Member More Info »
232.2R-03: Use of Fly Ash in Concrete Topic: Fly Ash Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 232 Published: 3/2004 Regular Price: $ 65.50 USD Member Price: $ 40.00 USD Become a Member More Info »
228.1R-03: In-Place Methods to Estimate Concrete Strength Topic: Nondestructive Evaluation Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 228 Published: 11/2003 Regular Price: $ 70.50 USD Member Price: $ 44.00 USD Become a Member More Info »
225R-99: Guide to the Selection and Use of Hydraulic Cements(Reapproved 2009) Topic: Cementitious Materials Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 225 Published: 1/2017 Regular Price: $ 37.50 USD Member Price: $ 25.00 USD Become a Member More Info »
225R-16 Guide to the Selection and Use of Hydraulic Cements Topic: Cementitious Materials Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 225 Published: 8/2016 Regular Price: $ 70.50 USD Member Price: $ 44.00 USD Become a Member More Info »
222R-01: Protection of Metals in Concrete Against Corrosion (Reapproved 2010) Topic: Corrosion Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 222 Published: 8/2002 Regular Price: $ 61.50 USD Member Price: $ 38.00 USD Become a Member More Info »
216.1M-07 Code Requirements for Determining Fire Resistance of Concrete and Masonry Construction Assemblies (Metric) Topic: Codes , Fire Resistance Format: PDF Unit: SI: International System of Units Language: English Author: Joint ACI/TMS Comm 216 Published: 11/2008 Regular Price: $ 59.50 USD Member Price: $ 37.00 USD Become a Member More Info »
214.3R-88: Simplified Version of the Recommended Practice for Evaluation of Strength Test Results of Concrete (Reapproved 1997) Topic: Testing Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 214 Published: 8/2002 Regular Price: $ 26.50 USD Member Price: $ 19.00 USD Become a Member More Info »
212.3R-10 Report on Chemical Admixtures for Concrete Topic: Admixtures Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 212 Published: 1/2017 Regular Price: $ 91.50 USD Member Price: $ 57.00 USD Become a Member More Info »
211.2-98: Standard Practice for Selecting Proportions for Structural Lightweight Concrete (Reapproved 2004) Topic: Mixture Proportioning Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 211 Published: 8/2002 Regular Price: $ 36.50 USD Member Price: $ 21.00 USD Become a Member More Info »
210R-93: Erosion of Concrete in Hydraulic Structures (Reapproved 2008) Topic: Hydraulic Structures Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 210 Published: 8/2002 Regular Price: $ 52.50 USD Member Price: $ 33.00 USD Become a Member More Info »
207.4R-05: Cooling and Insulating Systems for Mass Concrete (Reapproved 2012) Topic: Mass Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 207 Published: 10/2005 Regular Price: $ 52.50 USD Member Price: $ 33.00 USD Become a Member More Info »
207.3R-94: Practices for Evaluation of Concrete in Existing Massive Structures for Service Conditions (Reapproved 2008) Topic: Mass Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 207 Published: 8/2002 Regular Price: $ 60.50 USD Member Price: $ 37.00 USD Become a Member More Info »