548.6R-96: Polymer Concrete-Structural Applications State-of-the-Art-Report

Currency Display

Your Price: $ 47.50 USD

Member Price: $ 31.00 USD

Save $ 16.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**A newer version of this document exists**

NEW VERSION

 

Description

Polymer concrete (PC) is used in the construction of structural elements. Applications include wall panels to carry wind and seismic loads; underground vaults that must resist lateral earth pressure; vault and utility box covers that are required to resist vehicle loads; machine tool components subject to a wide range of loadings; and railroad ties to resist static and dynamic rail loads. Structural uses of PC components involve flexure, shear, bearing, and deflections. Creep, fatigue, and service temperature are important aspects of these mechanisms. A need for defining and understanding polymer concrete's structural properties and behavior therefore exists. Standards and codes governing design with polymer concrete have not yet been developed.

 

Document Details

Author: ACI/ V. M. Malhotra

Publication Year: 2002

Pages: 23

ISBN: 9780870315367

Categories: Polymer Concrete

Formats: PDF

This document is Historical

Table of Contents

Chapter 1 - Historic Development

Chapter 2 - Materials and Properties

*Materials for structural polymer concrete

*Polymer concrete types

*Mechanical properties

*Chemical and physical characteristics

*Standards and guides applicable to polymer concrete

*Safety

*Regulatory matters

*Materials research

*Suggested additional research

Chapter 3 - Structural Members

*Flexural members

*Compression members

*Reinforced polymer concrete

*Unreinforced polymer concrete

*Sandwich panels

Chapter 4 - Applications in structures

*Architectural panels and facades

*Transportation

*Electrical insulators

*Utility structures

*Hydraulic structures

*Hazardous waste containment

*Machine tools

Chapter 5 - Glossary of terms

Chapter 6 - References

*Recommended references

*Reference organizations

*Cited references

Appendix 1

Appendix 2

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.