548.8M-07 Specification for Type EM (Epoxy Multi-Layer) Polymer Overlay for Bridge and Parking Garage Decks (Metric)

548.8M-07 Specification for Type EM (Epoxy Multi-Layer) Polymer Overlay for Bridge and Parking Garage Decks (Metric)

Currency Display

Your Price:$ 36.50 USD

Member Price: $ 24.00 USD

Save $ 12.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**A newer version of this document exists**

NEW VERSION

 

Description

This Specification covers epoxy multi-layer (EM) polymer overlays for bridge and parking garage decks. Type EM polymer overlays incorporate a low-modulus epoxy binder and selected aggregate to produce a flexible, skid-resistant, and waterproof overlay. The overlay may be used for both new construction and rehabilitation. The overlay is placed by applying the neat epoxy binder to the surface and broadcasting aggregate. This Specification includes requirements for chemical components, aggregates, storage and handling, surface preparation, surface profile, mixing, placement, and finishing.

Keywords: bridge decks; epoxy; multi layer; overlays, polymer; parking garage decks; surface preparation.

 

Document Details

Author: ACI Committee 548

Publication Year: 2007

ISBN: 9780870312618

Categories: Polymer Concrete

Formats: PDF

This document is Historical

Table of Contents

Section 1 - General

1.1 Scope

1.2 Reference Standards

1.3 Reference Organizations

1.4 Submittals

1.5 Polymer conditions

1.6 Labeling, storage, and handling of materials

1.7 Safety

Section 2 - Products

2.1 Epoxy binder

2.2 Aggregate

2.3 Polymer Overlay

Section 3 - Execution

3.1 Procedure qualification

3.2 Surface preparation

3.3 Mixing epoxy binder

3.4 Overlay application

3.5 Curing

3.6 Excess aggregate removal

3.7 Joints

3.8 Open to traffic

Foreword to checklists

Mandatory Requirements checklist

Submittal checklist

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).