ACI PRC-544.5-10: Report on the Physical Properties and Durability of Fiber-Reinforced Concrete

Currency Display

Your Price: $ 68.50 USD

Member Price: $ 44.00 USD

Save $ 24.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Preview

Description

This document addresses the physical properties and durability of fiber-reinforced concrete (FRC). The effects of fiber reinforcement are evaluated for various physical, short-term, and long-term benefits they impart to the concrete mixture. A variety of test methods, conditions, and properties are reported. The various properties listed, in addition to the wide variety of the choices available in formulating matrix systems, allow performance-based specification of concrete materials using fibers to become a viable option. This document provides a historical basis and an overview of the current knowledge of FRC materials for tailoring new, sustainable, and durable concrete mixtures.

This document is divided into three sections. The first section discusses the physical properties of FRC in terms of electrical, magnetic, and thermal properties. Rheological properties, which affect fiber dispersion and distribution, are discussed using both empirical and quantitative rheology. Mechanisms of creep and shrinkage and the role of various fiber types in affecting both plastic shrinkage cracking and restrained shrinkage cracking are also addressed. The durability of concrete as affected by the addition of fibers is documented under freezing and thawing, corrosion resistance, and scaling. The durability of FRC systems is also affected as different fibers respond differently to the highly alkaline cementitious microstructure. The durability of alkali-resistant glass and cellulose fibers are studied by an in-depth evaluation of long-term accelerated aging results. Degradation and embrittlement due to alkali attack and bundle effect are discussed. Recent advances for modeling and design of materials with aging characteristics are presented. Literature on the use of FRC materials under aggressive environments, extreme temperatures, and fire is presented. The final sections list a series of applications where the use of FRC has resulted in beneficial durability considerations.

Keywords: aging; chloride permeability; corrosion; cracking; creep; diffusion; degradation; ductility; durability; electric properties; embrittlement; fiberreinforced cement-based materials; fiber-reinforced products; fire resistance; flexural strength; freezing-and-thawing; glass; microcracking; permeability; plastic shrinkage; polypropylene; polyvinyl alcohol; reinforcing materials; rheology; shrinkage cracking; steel; sulfate attack; thermal conductivity; toughness; water permeability; wood pulp.

 

Document Details

Author: ACI Committee 544

Publication Year: 2010

Pages: 31

ISBN: 9780870313653

Categories: Fiber-Reinforced Concrete

Formats: PDF

Table of Contents

Chapter 1—Introduction and scope

1.1—Introduction

1.2—Scope

Chapter 2—Notation, definitions, and acronyms

2.1—Notation

2.2—Definitions

2.3—Acronyms

Chapter 3—Physical properties of fiber-reinforced concrete (FRC)

3.1—Creep

3.2—Shrinkage

3.3—Permeability and diffusion

3.4—Rheology

3.5—Electrical properties

3.6—Thermal conductivity

Chapter 4—Durability of FRC

4.1—Extreme temperature and fire

4.2—Freezing and thawing

4.3—Degradation and embrittlement due to alkali attack

and bundle effect

4.4—Weathering and scaling

4.5—Corrosion resistance

Chapter 5—Applications and durability-based design

5.1—Case studies of applications of FRC materials and durability

Chapter 6—References

6.1—Referenced standards and reports

6.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.