ACI PRC-351.2-10 Report on Foundations for Static Equipment (Reapproved 2020)

Currency Display

Your Price: $ 54.50 USD

Member Price: $ 34.00 USD

Save $ 20.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Preview

Description

This document addresses static equipment foundation engineering and construction. It presents various design criteria, methods and procedures of analysis, design, and construction applied to static equipment foundations by industry practitioners. This document should, hopefully, encourage discussion and comparison of ideas.

Keywords: anchorage (structural); bolts, anchor; equipment; forms; formwork (construction); foundation loading; foundations; grout; grouting; pedestals; pile loads; reinforcement; soil pressure; subsurface preparation;tolerances (mechanics).

 

Document Details

Author: ACI Committee 351

Publication Year: 2010

Pages: 26

ISBN: 9780870313721

Categories: Foundations

Formats: PDF

Table of Contents

Chapter 1—Introduction and scope

1.1—Background

1.2—Purpose

1.3—Scope

Chapter 2—Notation and definitions

2.1—Notation

2.2—Definitions

Chapter 3—Foundation types

3.1—General considerations

3.2—Typical foundations

Chapter 4—Design criteria

4.1—Foundation loading

4.2—Design strength/stresses

4.3—Stiffness/deflections

4.4—Stability

Chapter 5—Design methods

5.1—Available methods

5.2—Anchor bolts and shear devices

5.3—Bearing stress

5.4—Pedestals

5.5—Soil pressure

5.6—Pile loads

5.7—Foundation design procedures

Chapter 6—Construction considerations

6.1—Subsurface preparation and improvement

6.2—Foundation placement tolerances

6.3—Forms and shores

6.4—Sequence of construction and construction joints

6.5—Equipment installation and setting

6.6—Grouting

6.7—Concrete materials

6.8—Quality control

Chapter 7—References

7.1—Referenced standards and reports

7.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.