Concrete mixtures intended for pavements have purposes and desired characteristics that are different from other types of mixtures, such as structural or mass concrete. Thus, a guide for designing concrete mixtures specific to paving, such as highways, streets, airfields, and parking lots, is necessary. This guide describes a method for designing mixtures and selecting trial mixture proportions for hydraulic-cement concrete made with and without supplementary cementitious materials, chemical admixtures, and fibers. The guide provides a method that focuses on designing the concrete mixture in the context of pavement structural design, concrete production, construction operations, and the environment in which the pavement will reside. Trial mixture proportions are for concrete consisting of normalweight aggregates and concrete with workability suitable for various types of pavement construction, such as slipform, fixed-form, and laser-guided screeding. The method provides an initial approximation of proportions intended to be analyzed to assess their performance potential for mixing, transporting, placing, screeding and consolidating, finishing, texturing, and time-of-setting. The method also considers the hardened concrete performance parameters of strength, durability, abrasion resistance, skid resistance, smoothness, and dimensional and shape stability. Methods of checking for incompatibilities of materials in given construction environments are included, as well as methods for aggregate grading optimization. Resulting proportions should be checked by preparing and analyzing trial mixtures in the laboratory, then in the field, and adjusting as necessary to produce the desired concrete characteristics. Special concrete pavement mixtures, such as pervious concrete or roller-compacted concrete, are not included in the document. This is a dual-unit document; however, paired values stated in inch-pound and SI units are usually not exact equivalents. Therefore, either system should be used independently of the other.

Keywords: aggregate optimization; aggregates; cementitious materials; fly ash; incompatibility; intermediate aggregate; mixture proportioning; mixtures; pavements; slag cement.

 

Document Details

Author: ACI Committee 325

Publication Year: 2017

Pages: 72.00

ISBN: 9781945487668

Categories: Pavements

Formats: Printed Document, PDF, ePub, or Kindle

Table of Contents

CHAPTER 1—INTRODUCTION

1.1—General

1.2—Mixture design goals

CHAPTER 2—NOTATION AND DEFINITIONS

2.1—Notation

2.2—Definitions

CHAPTER 3—BASIC PROPERTIES

3.1—Desired properties

3.2—Workability

3.3—Strength

3.4—Durability

3.5—Skid resistance

3.6—Smoothness

3.7—Dimensional and shape stability

3.8—Time of setting

3.9—Basic properties and considerations

3.10—Sustainability

3.11—Innovative methods and materials

CHAPTER 4—MATERIALS

4.1—Aggregate

4.2—Portland cement

4.3—Supplementary cementitious materials

4.4—Blended cement

4.5—Water

4.6—Chemical admixtures

4.7—Fibers

4.8—Summary

CHAPTER 5—MIXTURE PROPORTIONING

5.1—Mixture design

5.2—Proportioning methods

5.3—Preliminary testing

5.4—Proportioning procedure

CHAPTER 6—SAMPLE MIXTURE DESIGNS

6.1—Example 1: Urban highway, slipform, traditional grading, no SCMs (U.S. customary units)

6.2—Example 2: Urban highway, slipform, optimized grading, Class C fly ash (U.S. customary units)

6.3—Example 3: City street, fixed-form, optimized grading, sulfate soil, slag cement (U.S. customary units)

6.4—Example 4: Airfield, slipform, traditional grading, alkali-silica reaction aggregate, Class F fly ash (U.S. customary units)

6.5—Example 5: Parking lot, laser-guided screed, optimized grading, fibers (U.S. customary units)

6.6—Example 6: Urban highway, slipform, traditional grading, no SCMs (SI units)

CHAPTER 7—REFERENCES

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).