ACI PRC-304.2-17: Guide to Placing Concrete by Pumping Methods

Price: $ 54.50 USD

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Preview

Description

This guide discusses the use of pumps for transporting and placing concrete. Rigid and flexible pipelines, couplings and other accessories, and the various types of concrete pumps are discussed. The importance of proportioning a pumpable concrete mixture is emphasized with reference to sources for further direction on its design. Evaluation of trial mixtures to ensure pumpability and strength is encouraged. Of specific importance is a discussion on the use of lightweight aggregates. Methods to saturate these aggregates and provide a consistent moisture content are discussed.

Preconstruction planning for equipment placement and line routing are emphasized. Discussions on achieving a consistent mixture and its critical importance are also addressed.

Keywords: blockage; boundary layer; concrete pump; coupling; mixture design; pipeline; placing boom; preprimed; pumpability; reverse pumping; valve.

 

Document Details

Author: ACI Committee 304

Publication Year: 2017

ISBN: 9781945487828

Formats: PDF

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE

1.1—Introduction

1.2—Scope

CHAPTER 2—DEFINITIONS

CHAPTER 3—PUMPING CONCRETE

3.1—Mixture component distribution

3.2—Disruptions to flow

CHAPTER 4—PUMPING EQUIPMENT AND COMPONENTS

4.1—Piston pumps

4.2—Valve types

4.3—Trailer pumps

4.4—Truck-mounted concrete pumps

4.5—Separate placing booms

4.6—Specialized equipment

4.7—Pipeline and accessories

4.8—Flexible system hose types and applications

4.9—Concrete placing system accessories

CHAPTER 5—PUMPABLE CONCRETE

5.1—Basic considerations

5.2—Normalweight aggregate

5.3—Lightweight aggregate concrete

5.4—Water and slump

5.5—Cementitious materials

5.6—Admixtures

5.7—Fiber reinforcement

5.8—Trial mixtures and pumpability testing

5.9—Estimating performance

CHAPTER 6—FIELD PRACTICES

6.1—General

6.2—Pipeline concrete placement

6.3—Powered boom placement

6.4—Equipment and operational safety

6.5—Reduction in air content

CHAPTER 7—FIELD CONTROL

CHAPTER 8—REFERENCES

Authored documents

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.