On-Demand Course: Quality Management: The Common Thread of Good Practice (Part 2) Topic: Design , Inspection , Quality Assurance , Testing Format: Online Learning Unit: IN-LB: Inch-Pound Units Language: English Author: Hausfeld, Mehta, Lines Published: 4/2021 Price:$ 39.00 USD Become a Member More Info »
ACI PRC-211.6-14: TechNote: Aggregate Suspension Mixture Proportioning Method Topic: Mixture Proportioning Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 211 Published: 12/2014 Price:$ 19.00 USD Become a Member More Info »
SP-217: Seventh CANMET/ACI International Conference on Superplasticizers and Other Chemical Admixtures in Concrete Topic: Admixtures Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 9/2003 Regular Price: $ 125.50 USD Member Price: $ 76.00 USD Become a Member More Info »