ACI PRC-440-07 Report on Fiber-Reinforced Polymer (FRP) Reinforcement for Concrete Structures Topic: Fiber-Reinforced Concrete Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 440 Published: 9/2007 Price:$ 99.50 USD Become a Member More Info »
ACI PRC-544.7-16 Report on Design and Construction of Fiber-Reinforced Precast Concrete Tunnel Segments Topic: Fiber-Reinforced Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 2/2016 Price:$ 86.50 USD Become a Member More Info »
MNL-7(23) GFRP-Reinforced Concrete Design Handbook Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI/NEx Published: 12/2023 Regular Price: $ 149.00 USD Member Price: $ 89.00 USD Become a Member More Info »
ACI PRC-544.4-18: Guide to Design with Fiber-Reinforced Concrete Topic: Fiber-Reinforced Concrete Format: Printed Document or PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 7/2018 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-544.9-17: Report on Measuring Mechanical Properties of Hardened Fiber-Reinforced Concrete Topic: Fiber-Reinforced Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 1/2017 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-549.4-20: Guide to Design and Construction of Externally Bonded Fabric-Reinforced and Steel-Reinforced Grout Systems for Repair and Strengthening of Concrete Structures Topic: Bonded , Fiber-Reinforced Concrete , Post Tensioning , Reinforcement Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 549 Published: 4/2020 Price:$ 54.00 USD Become a Member More Info »
SPEC-544.12-23: Performance-Based Fiber-Reinforced Concrete for Slabs-on-Ground and Overlays—Specification Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 544 Published: 12/2023 Regular Price: $ 54.00 USD Member Price: $ 34.00 USD Become a Member More Info »
ACI PRC-544.10-21: Fiber Effect on Reducing the Permeability of Cracked Concrete Structures—TechNote Topic: Cracking , Durability , Fiber-Reinforced Concrete Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 544 Published: 6/2021 Price:$ 19.00 USD Become a Member More Info »
The Contractor's Guide to Quality Concrete Construction - Third Edition Spanish Version Topic: Construction Practices Format: Unit: IN-LB: Inch-Pound Units Language: Spanish Published: 9/2011 Regular Price: $ 94.00 USD Member Price: $ 64.00 USD Become a Member More Info »
ACI PRC-440.1-15 Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer Bars Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English or Spanish Author: ACI Committee 440 Published: 10/2021 Price:$ 113.50 USD Become a Member More Info »
ACI PRC-544.3-08: Guide for Specifying, Proportioning, and Production of Fiber-Reinforced Concrete Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 11/2008 Price:$ 50.50 USD Become a Member More Info »
ACI PRC-544.11-22: Measuring Shrinkage, Creep, and Transport Properties of Fiber-Reinforced Concrete—Report Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 7/2022 Regular Price: $ 54.00 USD Member Price: $ 34.00 USD Become a Member More Info »
ACI PRC-360-10 Guide to Design of Slabs-on-Ground Topic: Slabs Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 360 Published: 4/2010 Price:$ 105.00 USD Become a Member More Info »
ACI CODE-440.11-22: Building Code Requirements for Structural Concrete Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars—Code and Commentary Topic: Codes Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units or SI: International System of Units Language: English Author: ACI Committee 440 Published: 3/2023 Regular Price: $ 155.00 USD Member Price: $ 95.00 USD Become a Member More Info »
ACI PRC-440.7-22: Externally Bonded Fiber-Reinforced Polymer Systems Design and Construction for Strengthening Masonry Structures - Guide Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 440 Published: 1/2023 Price:$ 54.00 USD Become a Member More Info »