ACI PRC-304.3-20: Heavyweight Concrete: Measuring, Mixing, Transporting and Placing Topic: Admixtures , Aggregates , Consolidation , Formwork , Grouting , Materials Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 304 Published: 8/2020 Price:$ 54.00 USD Become a Member More Info »
ACI PRC-447.1-18: Report on the Modeling Techniques Used in Finite Element Simulations of Concrete Structures Strengthened Using Fiber-Reinforced Polymer (FRP) Materials Topic: Fiber-Reinforced Concrete Format: Printed Document or PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 447 Published: 9/2018 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-549.1-18: Design Guide for Ferrocement Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 549 Published: 9/2018 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-306-16 Guide to Cold Weather Concreting Topic: Cold Weather Format: Printed Document, Protected PDF/Web View, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 306 Published: 8/2016 Price:$ 75.00 USD Become a Member More Info »
ACI PRC-549.6-20: Guide to Design and Construction of Externally Bonded Fabric-Reinforced Cementitious Matrix (FRCM) and Steel-Reinforced Grout (SRG) Systems for Repair and Strengthening Masonry Structures Topic: Design , Masonry , Repair Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 549 Published: 11/2020 Price:$ 54.00 USD Become a Member More Info »
MNL-15(20): Field Reference Manual Topic: Specifications Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: American Concrete Institute Published: 10/2020 Regular Price: $ 249.00 USD Member Price: $ 199.00 USD Become a Member More Info »
ACI PRC-228.1-19: Report on Methods for Estimating In-Place Concrete Strength Topic: Nondestructive Evaluation Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 228 Published: 1/2019 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-325.10-95: Report on Roller-Compacted Concrete Pavements (Reapproved 2001) - Spanish Language Format: PDF Unit: IN-LB: Inch-Pound Units Language: Spanish Author: Translated by: ICCYC Published: 12/2014 Regular Price: $ 67.50 USD Member Price: $ 41.00 USD Become a Member More Info »
ACI PRC-214S-11 Guide to Evaluation of Strength Test Results of Concrete - Spanish Language Topic: Testing Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: Spanish Author: ACI Committee 214 Published: 1/2017 Price:$ 59.50 USD Become a Member More Info »
MNL-2(19): Manual of Concrete Inspection, 11th Edition Topic: Inspection Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 311 Published: 2/2019 Regular Price: $ 149.00 USD Member Price: $ 95.00 USD Become a Member More Info »
ACI PRC-325.11-19: Report on Accelerated Techniques for Concrete Paving Topic: Pavements Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 325 Published: 3/2019 Price:$ 49.50 USD Become a Member More Info »
ACI PRC-364.7-21: Evaluation and Minimization of Bruising in Concrete Repair - TechNote Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 364 Published: 8/2021 Price:$ 19.00 USD Become a Member More Info »
ACI PRC-350.2-21: Hazardous Material Containment in Concrete Structures - Report Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 350 Published: 10/2021 Regular Price: $ 54.00 USD Member Price: $ 34.00 USD Become a Member More Info »
ACI PRC-363.2-11 Guide to Quality Control and Assurance of High-Strength Concrete Topic: High Performance Concrete Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 363 Published: 7/2011 Price:$ 63.50 USD Become a Member More Info »
ACI PRC-207.3-18: Report on Practices for Evaluation of Concrete in Existing Massive Structures for Service Conditions Topic: Mass Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 207 Published: 1/2018 Price:$ 54.50 USD Become a Member More Info »