ACI PRC-325.14-17: Guide for Design and Proportioning of Concrete Mixtures for Pavements Topic: Pavements Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 325 Published: 6/2017 Price:$ 60.50 USD Become a Member More Info »
ACI PRC-544.1R-96: Report on Fiber Reinforced Concrete (Reapproved 2009) Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 9/2002 Price:$ 79.50 USD Become a Member More Info »
ACI PRC-549.3-22: Glass Fiber-Reinforced Concrete Premix—Report Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 549 Published: 9/2022 Price:$ 54.00 USD Become a Member More Info »
ACI PRC-357-84: Guide for the Design and Construction of Fixed Offshore Concrete Structures (Reapproved 1997) Topic: Marine Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 357 Published: 8/2002 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-232.2-18: Report on the Use of Fly Ash in Concrete Topic: Fly Ash Format: Printed Document or PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 232 Published: 4/2018 Price:$ 64.50 USD Become a Member More Info »
SP-017(14): The Reinforced Concrete Design Handbook Volumes 1 & 2 Package Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Published: 11/2014 Regular Price: $ 209.50 USD Member Price: $ 129.00 USD Become a Member More Info »
ACI PRC-213S-03 Guide for Structural Lightweight-Aggregate Concrete - Spanish Version Topic: Lightweight Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: Spanish Published: 12/2014 Price:$ 63.50 USD Become a Member More Info »
SP-017(14): The Reinforced Concrete Design Handbook (Metric) Faculty Network Format: Protected PDF/Web View Unit: SI: International System of Units Language: English Published: 5/2018 Regular Price: $ 0.00 USD Member Price: $ 0.00 USD Become a Member More Info »
SP-017(14): The Reinforced Concrete Design Handbook (Metric) Topic: Design Format: Protected PDF/Web View Unit: SI: International System of Units Language: English Published: 5/2018 Regular Price: $ 204.00 USD Member Price: $ 124.00 USD Become a Member More Info »
ACI PRC-365.1-17: Report on Service Life Prediction Format: Printed Document or PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 365 Published: 10/2017 Price:$ 74.50 USD Become a Member More Info »
ACI PRC-440.2-23: Design and Construction of Externally Bonded Fiber-Reinforced Polymer (FRP) Systems for Strengthening Concrete Structures—Guide Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 440 Published: 11/2023 Price:$ 99.00 USD Become a Member More Info »
ACI PRC-440-07 Report on Fiber-Reinforced Polymer (FRP) Reinforcement for Concrete Structures Topic: Fiber-Reinforced Concrete Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 440 Published: 9/2007 Price:$ 99.50 USD Become a Member More Info »
MNL-3(16) Guide to the Code for Assessment, Repair, and Rehabilitation of Existing Concrete Buildings Topic: Codes , Repair Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Published: 9/2016 Regular Price: $ 135.00 USD Member Price: $ 79.00 USD Become a Member More Info »
ACI PRC-234-06: Guide for the Use of Silica Fume in Concrete (Reapproved 2012) Topic: Silica Fume Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 234 Published: 6/2006 Price:$ 88.50 USD Become a Member More Info »
MNL-17(21) - ACI Reinforced Concrete Design Handbook Topic: Cracking , Design , Post Tensioning , Reinforcement , Slabs Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: American Concrete Institute Published: 3/2021 Regular Price: $ 249.00 USD Member Price: $ 159.00 USD Become a Member More Info »