ACI PRC-308S-01 Guide to Curing Concrete - Spanish Language Topic: Curing Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: Spanish Author: Translated by: IMCYC Published: 7/2014 Price:$ 60.50 USD Become a Member More Info »
ACI PRC-304-00: Guide for Measuring, Mixing, Transporting, and Placing Concrete (Reapproved 2009) Topic: Placing Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 304 Published: 8/2002 Price:$ 104.50 USD Become a Member More Info »
ACI PRC-343-95: Analysis & Design of Reinforced Concrete Bridge Structures (Repproved 2004) Topic: Bridges Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 341 Published: 8/2002 Price:$ 160.50 USD Become a Member More Info »
ACI PRC-224.3-95: Joints in Concrete Construction (Reapproved 2013) Topic: Joints - Movement Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 224 Published: 8/2002 Price:$ 101.50 USD Become a Member More Info »
ACI PRC-302.2-22: Concrete Slabs that Receive Moisture-Sensitive Flooring Materials - Guide Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 302 Published: 2/2023 Regular Price: $ 85.00 USD Member Price: $ 49.00 USD Become a Member More Info »
ACI PRC-130-19: Report on the Role of Materials in Sustainable Concrete Construction Topic: Sustainability Format: Printed Document or PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 130 Published: 1/2019 Price:$ 54.00 USD Become a Member More Info »
ACI PRC-345-91: Guide for Concrete Highway Bridge Deck Construction (Reapproved 2005) - Spanish Language Topic: Bridges Format: PDF Unit: IN-LB: Inch-Pound Units Language: Spanish Author: Translated by: ICCYC Published: 12/2014 Regular Price: $ 62.50 USD Member Price: $ 35.00 USD Become a Member More Info »
ACI CODE-376-23: Refrigerated Liquefied Gas Containment for Concrete Structures—Code Requirements and Commentary Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 376 Published: 7/2023 Regular Price: $ 131.50 USD Member Price: $ 79.00 USD Become a Member More Info »
ACI PRC-306-16 Guide to Cold Weather Concreting Topic: Cold Weather Format: Printed Document, Protected PDF/Web View, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 306 Published: 8/2016 Price:$ 75.00 USD Become a Member More Info »
ACI PRC-544.2-17: Report on the Measurement of Fresh State Properties and Fiber Dispersion of Fiber-Reinforced Concrete Topic: Fiber-Reinforced Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 5/2017 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-305-20: Guide to Hot Weather Concreting Topic: Curing , Hot Weather Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 305 Published: 10/2020 Price:$ 95.00 USD Become a Member More Info »
ACI PRC-357.2-10 Report on Floating and Float-In Concrete Structures Topic: Marine Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 357 Published: 7/2010 Price:$ 76.50 USD Become a Member More Info »
ACI PRC-215-21: Concrete Structure Design for Fatigue Loading—Report Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 215 Published: 4/2022 Price:$ 54.00 USD Become a Member More Info »
ACI PRC-522-23: Pervious Concrete—Report Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 522 Published: 6/2023 Price:$ 54.00 USD Become a Member More Info »
MNL-15(20): Field Reference Manual Topic: Specifications Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: American Concrete Institute Published: 10/2020 Regular Price: $ 249.00 USD Member Price: $ 199.00 USD Become a Member More Info »