201.2R-08: Guide to Durable Concrete Topic: Durability Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 201 Published: 5/2008 Regular Price: $ 80.50 USD Member Price: $ 51.00 USD Become a Member More Info »
117-90: Standard Specifications for Tolerances for Concrete Construction and Materials (Reapproved 2002) Topic: Tolerances Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 117 Published: 8/2002 Regular Price: $ 26.50 USD Member Price: $ 17.00 USD Become a Member More Info »
117-06 Specifications for Tolerances for Concrete Construction and Materials and Commentary Topic: Tolerances Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 117 Published: 10/2006 Regular Price: $ 81.50 USD Member Price: $ 49.00 USD Become a Member More Info »
104-71: Preparation of Notation for Concrete (Revised 1982) (Reapproved 1997) Topic: Notation Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 104 Published: 8/2002 Regular Price: $ 29.50 USD Member Price: $ 19.00 USD Become a Member More Info »