On-Demand Course: Coarse and Fine Lightweight Aggregates for Use in Concrete

On-Demand Course: Coarse and Fine Lightweight Aggregates for Use in Concrete

Your Price: $30.00 USD

Member Price: $24.00 USD

Save $6.00 USD, Become a Member

Choose Product Language

Choose Product Format

Quantity:


Notes/Preview

INSTRUCTIONS: View the recorded webinar. Complete 10-question quiz with a score of 80% or higher to receive a certificate for 0.1 CEU (equivalent to 1.0 PDH).

Continuing Education Credit: 0.1 CEU (1.0 PDH)

Approved by AIA (LU/HSW) and ICC

Access Period: 30 days

Description

This is a recorded webinar from June 5, 2018.

Concrete mixtures can include lightweight coarse and/or lightweight fine aggregates. This presentation will explain the process of mining shale and expanding it into lightweight aggregate. Applications of products from expanded shale include bridge decks, slabs-on-deck in buildings, and internal curing. There is a section of the presentation that includes excerpts from the NYSDOT 2017 Bridge Manual that requires internal curing in the concrete for bridge decks, sidewalks, crash walls, and approach slabs. Also included are a few project profiles for bridge decks, concrete paving, and pervious concrete.

 

Document Details

Author: Ronald E. Vaughn

Publication Year: 2018

Pages: 0.00

ISBN:

Categories: Aggregates, Curing

Formats: Online Learning

Table of Contents

Learning Objectives:

1. Explain the process of mining and expanding shale into lightweight aggregate (LWA).

2. Describe the benefits of using LWA in concrete mixtures.

3. Identify the difference between absorbed and surface moisture in LWA.

4. Explain the mechanism and benefits of internal curing in concrete.

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).