SP-064: Cedric Willson Symposium on Expansive Cement

SP-064: Cedric Willson Symposium on Expansive Cement

Your Price: $84.75 USD

Member Price: $55.25 USD

Save $29.50 USD, Become a Member

Choose Product Language

Choose Product Format


Notes/Preview

PURCHASE INDIVIDUAL PAPERS

Description

This symposium of 16 papers covers international developments, field service reports on existing installations and research. Reports on applications of shrinkage-compensating concrete in hydraulic structures, cold storage warehouse, slabs, bridge decks, oil well cementing, post-tensioned structures.

 

Document Details

Publication Year: 2002

Pages: 336.00

ISBN: 9780870317026

Categories: Expansive Cement

Formats: PDF

Table of Contents

- The Future of Expansive Cement, by Bryant Mather

- Hydraulic Structures Designed with Shrinkage-

Compensating Concrete, by Joe V. Williams, Jr.

- Utilization of Shrinkage-Compensating Concrete--A Cold

Storage Warehouse Application, by Charles A. Gaskill

and Richard C. Jacobs

- Use of Shrinkage-Compensating Cement Concrete in the

Dallas Municipal Center, by Jack E. Rosenlund

- Expansive Cement Concretes in Japan, by Shigeyoshi

Nagataki

- Performance of Shrinkage-Compensating Concretes in Slabs,

by H. G. Russell

- Tidal Exposure Effects on Concrete Made with Shrinkage

-Compensating Concrete, by G. B. Moore

- Expansion-Shrinkage, creep, and Elastic Modulus of

Shrinkage-Compensating Gap-Graded Concrete, by Shu-t'ien

and V. Ramakrishnan

- A Look at Type K Shrinkage-Compensating Cement Production

and Specifications, by George C. Hoff and Katharine Mather

- Summary Report on Type K. Shrinkage-Compensating Concrete

Bridge Deck Installations in the State of Ohio, by David O. Lower

- Shrinkage-Compensating Cements in Oil Well Cementing,

by D. G. Calvert

- Portland Cement Versus Expansive Cement in Post-Tensioned

Concrete Structures, by Mark W. Hoffman

- Field Study of Shrinkage-Compensating Cement Concrete,

by Frank A. Randall, Jr.

- Crack Control for Spillway Chute at Ririe Dam, by Richard

A. Kaden and E. K. Schrader

- Behavior of Shrinkage-Compensating Concretes Suitable

for Use in Bridge Decks, by Robert W. Cusick and Clyde E. Kesler

- Method of Estimating Expansive Strains Produced in Reinforced

Concrete Members Using Expansive Cement Concrete, by

Yukikazu Tsuji.

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).