SP-61: Ferrocement--Materials and Applications

SP-61: Ferrocement--Materials and Applications

Your Price: $32.95 USD

Member Price: $21.75 USD

Save $11.20 USD, Become a Member

Choose Product Language

Choose Product Format


Notes/Preview

PURCHASE INDIVIDUAL PAPERS

Description

The eleven papers include an historical overview of ferrocement, structural properties useful to engineers, laboratory tests, research on properties, and applications. A bibliography is included.

Document Details

Publication Year: 2002

Pages: 204.00

ISBN: 9780870317002

Categories: Ferrocement

Formats: PDF

Table of Contents

- Ferrocement--Past and Present, by Gajanan M. Sabnis

- Survey of Mechanical Properties of Ferrocement as a

Structural Material, by Gordon B. Batson, Gajanan M. Sabnis

and Antoine E. Naaman

- Design Predictions of Crack Widths in Ferrocement,

by Antoine E. Naaman

- Study of Tensile Cracks and Bond-Slip in Ferrocement,

by Ricardo P. Pama, Vorachai Intargumhaeng, and

Bishwendu K. Paul

- Development of Fibrous Ferrocement, by Maurice Atcheson

and Douglas Alexander

- Tentative Recommendations for the Construction of

Ferrocement Tanks, by S. P. Shah

- Grading Design of Sand for Ferrocement Mixes, by Z. Raichvarger

and M. Raphael

- Ferrocement Service Modules for Housing, by

A. G. Madhava Rao, D. S. Ramchandra Murthy, R. Jayaraman,

and G. Paul Joseph

- Applications of Ferrocement in Low-Cost Housing in Mexico,

by Jose Castro

- Corrugated Ferrocement Sheets, by P. Srinivasa Rao and

M. S. Mathews

- Research Needs and the Future of Ferrocement, by James

P. Romualdi

- Bibliography on Ferrocement--Materials and Applications,

by Gajanan M. Sabnis, Gordon B. Batson, Antoine E. Naaman, and

Ricardo P. Pama

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the Manual of Concrete Practice (MCP). For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).