238.2T-14 Concrete Thixotropy

238.2T-14 Concrete Thixotropy

Your Price: $ 14.00 USD

Member Price: $ 9.00 USD

Save $ 5.00 USD, Become a Member

Choose Product Language

Choose Product Format


Description

Fresh concrete can exhibit different rheological behavior when at rest than when flowing. This difference is due to thixotropy, which can have important consequences for formwork pressure, multi-lift casting, slip-form paving, pumping, and segregation resistance. This TechNote defines thixotropy and distinguishes it from other changes in rheological properties; discusses the origins of, test methods for measuring, and factors affecting thixotropy; and concludes with its applications.

Keywords: aggregate segregation; formwork pressure; plastic viscosity; pumpability; rheology; rheometer; static yield stress; thixotropy; yield stress.

TechNotes are a committee document that are narrowly focused, single-topic guides, usually practice oriented, that present a specific direction on a particular issue. ACI committee documents (including TechNotes) are reviewed and approved by ACI's Technical Activities Committee.

 

Document Details

Author: ACI Committee 238

Publication Year: 2014

Pages: 6.00

ISBN:

Categories: Materials

Formats: PDF

Table of Contents

Introduction

Description of thixotropy

Origins of thixotropy

Measuring thixotropy

Effects of concrete materials and temperature on thixotropy

Applications of thixotropy

Summary

Referenced standards and reports

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).