237R-07 Self-Consolidating Concrete (Reapproved 2019)

237R-07 Self-Consolidating Concrete (Reapproved 2019)

Currency Display

Your Price: $ 65.50 USD

Member Price: $ 41.00 USD

Save $ 24.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Description

Self-consolidating concrete (SCC) has been successfully used in many projects around the world and has made a major impact on concrete placement and construction economics. This report contains the current state of knowledge with respect to SCC. The information in this document is expected to inform concrete producers, users, and specifiers of SCC of known practices and processes. Because SCC is a viable solution to various concrete placement problems, ASTM has established Subcommittee C09.47, Self-Consolidating Concrete, to develop standard test methods for SCC.

Keywords: admixture; aggregate; air entrainment; bleeding; ement;consolidation; curing; placing; self-consolidating concrete; specification;viscosity, workability.

 

Document Details

Author: ACI Committee 237

Publication Year: 2007

Pages: 30

ISBN: 9780870312441

Categories: Consolidation

Formats: PDF

Table of Contents

Chapter 1—Introduction

1.1—Definition of self-consolidating concrete (SCC)

1.2—Advantages

1.3—Development history of SCC

1.4—Selected case studies

Chapter 2—Fresh properties

2.1—Terminology relative to SCC

2.2—Performance requirements of SCC

2.3—General

2.4—Characteristics

2.5—Target guidelines for fresh properties

2.6—Quality control

Chapter 3—Hardened properties

3.1—General

3.2—Mechanical properties

3.3—Long-term durability

3.4—Aesthetics

Chapter 4—Guide for selecting proportions for SCC

4.1—General

4.2—Performance requirements

4.3—Materials

4.4—Mixture proportioning procedure

4.5—Examples of SCC mixture proportions

Chapter 5—Production

5.1—General

5.2—Production issues that influence fresh SCC properties

5.3—Performance targets

5.4—Mock-up

5.5—Employee training

Chapter 6—Transport, placement, and finishing

6.1—General

6.2—Transport

6.3—Discharge of SCC for slabs or open-top molds for factory-type precast elements

6.4—Forms, element characteristics, and reinforcement

6.5—Placement techniques

6.6—Finishing

6.7—Curing

Chapter 7—SCC specification guidelines

7.1—Concrete materials

7.2—Execution

Chapter 8—Test methods

8.1—Measuring SCC characteristics

8.2—Slump flow

8.3—Visual stability index

8.4—T50

8.5—J-ring

8.6—L-box

8.7—Column segregation

8.8—Other tests

Chapter 9—References

9.1—Referenced standards and reports

9.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.