224.3RS-95 Joints in Concrete Construction - Spanish Language
224.3RS-95 Juntas en las construcciones de concreto, versión en español

Currency Display

Your Price: $ 101.50 USD

Member Price: $ 59.00 USD

Save $ 42.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

This is a licensed translation and has not been reviewed or approved by ACI.

Preview


Description

This report reviews the state of the art in design, construction, and maintenance of joints in concrete structures subjected to a wide variety of use and environmental conditions. In some cases, the option of eliminating joints is considered Aspects of various joint sealant materials and jointing techniques are discussed. Chapters in the report focus on various types of structures and structural elements with unique characteristics: Buildings, bridges, slabs-on-grade, tunnel linings, canal linings, precast concrete pipe, liquid-retaining structures, walls, and mass concrete.

Keywords: bridges, buildings, canal linings, canals, concrete construction, construction joints, contraction joints, design, environmental engineering concrete structures, isolation joints, joints, parking lots, pavements, runways, slabs-on-trade, tunnel linings, tunnels, walls.

 

Document Details

Author: Translated by: IMCYC

Publication Year: 2015

ISBN: 9684641249

Categories: Joints - Movement

Formats: PDF

Table of Contents

Chapter 1 - Introduction

1.1-Joints in concrete structures

1.2-Joint terminology

1.3-Movement in concrete structures

1.4-Objectives and scope

Chapter 2 - Sealant materials and jointing techniques

2.1-Introduction

2.2-Required properties of joint sealants

2.3-Commercially available materials

2.4-Field-molded sealants

2.5-Accessory materials

2.6-Preformed sealants

2.7-Compression seals

2.8-Jointing practice

Chapter 3 - Buildings

3.1-Introduction

3.2-Construction joints

3.3-Contraction joints

3.4-Isolation or expansion joints

Chapter 4 - Bridges

4.1-Introduction

4.2-Construction joints

4.3-Bridges with expansion joints

4.4-Bridges without expansion joints

Chapter 5 - Slabs on grade

5.1-Introduction

5.2-Contraction joints

5.3-Isolation or expansion joints

5.4-Construction joints

5.5-Special considerations

Chapter 6 - Pavements

6.1-Introduction

6.2-Contraction joints

6.3-Isolation or expansion joints

6.4-Construction joints

6.5-Hinge or warping joints

6.6-Parking lots

Chapter 7 - Tunnels, canal linings and pipes

7.1-Introduction

7.2-Concrete tunnel linings

7.3-Concrete canal linings

7.4-Concrete pipe

Chapter 8 - Walls

8.1-Introduction

8.2-Types of joints in concrete walls

8.3-Contraction joints

8.4-Isolation or expansion joints

8.5-Construction joints

Chapter 9 - Liquid-retaining structures

9.1-Introduction

9.2-Contraction joints

9.3-Isolation or expansion joints

9.4-Construction joints

Chapter 10 - Mass concrete

10.1-Introduction

10.2-Contraction joints

10.3-Construction joints

Chapter 11 - References

11.1-Recommended references

11.2-Cited references

Appendix A - Temperatures used for calculation of T

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.