ACI PRC-222-19: Guide to Protection of Metals in Concrete Against Corrosion

Price: $ 54.50 USD

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Preview

Description

This guide reviews the most recent developments of metal corrosion, specifically reinforcing steel, in concrete. Individual chapters are devoted to corrosion of metals in concrete, protective measures for new concrete construction, procedures for identifying corrosive environments, active corrosion in concrete, and remedial measures.

Keywords: allowable chloride; carbonation; chloride; chloride threshold; corrosion; corrosion-resistant reinforcement; durability; prestressed concrete; reinforced concrete; reinforcing steels.

 

Document Details

Author: ACI Committee 222

Publication Year: 2019

Pages: 60

ISBN: 9781641950572

Categories: Corrosion

Formats: PDF

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE

1.1—Introduction

1.2—Scope

CHAPTER 2—NOTATION AND DEFINITIONS

2.1—Notation

2.2—Definitions

CHAPTER 3—MECHANISM OF CORROSION OF STEEL IN CONCRETE

3.1—Introduction

3.2—Principles of corrosion

3.3—Reinforcing bar

3.4—Concrete environment

CHAPTER 4—PROTECTION AGAINST CORROSION IN NEW CONSTRUCTION

4.1—Introduction

4.2—Design approaches and choices

4.3—Methods of excluding external sources of chloride from concrete

4.4—Corrosion control methods

4.5—Summary

CHAPTER 5—PROCEDURES FOR IDENTIFYING CORROSIVE ENVIRONMENTS AND ACTIVE CORROSION IN REINFORCED CONCRETE STRUCTURES

5.1—Introduction

5.2—Condition evaluation of reinforced concrete structures

5.3—Corrosion evaluation methods

5.4—Concrete evaluation test methods

CHAPTER 6—REMEDIAL MEASURES

6.1—Introduction

6.2—Applicability

6.3—Remedies and their limitations

6.4—Summary

CHAPTER 7—REFERENCES

Authored references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.