Statistical procedures provide valuable tools for evaluating the results of concrete strength tests. Information derived from such procedures is valuable in defining design criteria, specifications, and other parameters needed for structural evaluation and repair. This guide discusses variations that occur in concrete strength and presents statistical procedures useful in interpreting these variations with respect to specified testing and criteria.

Keywords: coefficient of variation; concrete strength; normal distribution;required overdesign; quality control; standard deviation; statistical methods.

 

Document Details

Author: ACI Committee 214

Publication Year: 2017

ISBN: 9781945487484

Categories: Testing

Formats: PDF

Table of Contents

Chapter 1—Introduction

1.1—Introduction

1.2—Summary

Chapter 2—Notation and definitions

2.1—Notation

2.2—Definitions

Chapter 3—Variations in strength

3.1—General

3.2—Influence of batch-to-batch variations on concrete strength

3.3—Influence of within-batch variations on concrete strength

Chapter 4—Analysis of strength data

4.1—General

4.2—Statistical functions

4.3—Strength variations

4.4—Interpretation of statistical parameters

4.5—Standards of control

Chapter 5—Criteria

5.1—General

5.2—Data used to establish minimum required average strength

5.3—Criteria for strength requirements

Chapter 6—Evaluation of data

6.1—General

6.2—Numbers of tests

6.3—Rejection of doubtful specimens

6.4—Additional test requirements

6.5—Quality-control charts

6.6—Additional evaluation techniques

Chapter 7—References

7.1—Referenced standards and reports

7.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).