Title: Proposed Specification for Concrete Pavements and Bases

Author(s): ACI Committee 617

Publication: Journal Proceedings

Volume: 40

Issue:

Appears on pages(s): 117-144

Keywords:

Date: 11/1/1943

Abstract:
These specifications apply to the construction of portland cement concrete pavement and base under normal conditions, including the preparation of the subgrade, and shall govern unless modified by special provisions to take into account unusual condi-tions of traffic, subgrade, drainage, exposure, and other factors. (Adopted by tne ACI convention, 1944, and ratified by letter ballot as an ACI Standard July 28, 1944).




  