Title: Field Survey Of Mass Concrete
Author(s): F. R. McMillan
Publication: Journal Proceedings
Volume: 34
Issue: 5
Appears on pages(s): 561-572
Keywords: none
Date: 5/1/1938
Abstract:
In this survey, Committee 108 attempts to determine to what extent the properties peculiar to mass concrete. are responsible for conditions observed massive structures. Effect of improved workmanship and changes in materials on properties of concrete are noted. These effects are demonstrated by descriptions of Crystal Springs, Elephant Butte, Arrow-rock, Morris, and Boulder dams, and others unidentified.