Title: Trends In The Production And Use Of Various Types Of Hydraulic Cements
Author(s): P. H. Bates
Publication: Journal Proceedings
Volume: 31
Issue: 11
Appears on pages(s): 225-240
Keywords: none
Date: 11/1/1934
Abstract:
The situation regarding the types of hydraulic cements on the market and the various service demands is reviewed. It is pointed out that the thought that one standard cement can be used to meet all commercial demands is rapidly being discarded. The nature of the cements available and some of their properties are briefly presented. The reasons why there is a demand for a variety of cements are discussed. are cautioned that all Producers and consumers t pes used successfully to make of cement may not be services.