Title: Architectural Concrete Of The Exposed Aggregate Type
Author(s): John J. Earley
Publication: Journal Proceedings
Volume: 30
Issue: 3
Appears on pages(s): 251-278
Keywords: none
Date: 3/1/1934
Abstract:
This paper is a continuation of "The Project of Ornamenting the Baha’i Temple Dome," ACI Journal, June 1933. Describes some of the techniques by which architectural concrete of the exposed age methods has been developed and some of the which the ornamentation of the Temple has been done.