Title: Simplified Concrete Mix Design

Author(s): H. N. Walsh

Publication: Journal Proceedings

Volume: 30

Issue: 11

Appears on pages(s): 110-120

Keywords: none

DOI: 10.14359/8302

Date: 11/1/1933

Abstract:
Contains grading curves of aggregates (both in. and 1 1/2 in. maximum sizes). Each grading makes dense and workable concrete with a specifiedproportion of cement. Corresponding water-cement ratios and cement contents of set concrete are given; cement-water ratio a straight line relation between included. by weight and strength is in-A simple method of proportioning from the above data is illustrated by an example.




  