Title: Guide for Construction of Concrete Floors on Grade

Author(s): ACI Committee 332

Publication: Journal Proceedings

Volume: 59

Issue: 10

Appears on pages(s): 1377-1390

Keywords: none

Date: 10/1/1962

Abstract:
This report of ACI Committee 332, Recommended Practice for Residential Concrete Work, was prepared to serve as a guide for the installation of concrete floor slabs on grade inside residences. The main concern of the com-mittee is one- and two-family dwelling construction. The report is not offered as a specification but as a guide to sound practices. The report is concerned with the requirements of the site; required quality of materials; mixing, placing, and curing the concrete; design of the slab; and special considerations as related to this particular type of construction.




  

Please enter this 5 digit unlock code on the web page.