Title: Dynamic Response of Pretensioned Prestressed Concrete Beams

Author(s): Wayne A. Hamilton

Publication: Journal Proceedings

Volume: 65

Issue: 10

Appears on pages(s): 851-855

Keywords: beams (structural);dynamic tests;loads (forces);prestressed concrete; pretensioning;research;testing;ultimate strength method (structural).

Date: 10/1/1968

Abstract:
Seven pretensioned concrete beams were subjected to a highly impulsive load. The load, reaction, and displacement of the member were recorded. A comparison is made by determining the ratio of ultimate dynamic moment to ultimate static moment. The test results show that the members will carry a 35 percent larger ultimate moment when applied dynamically.