Title: Splices and Anchorages in One-Way Slabs Reinforced with Deformed Wire Fabric

Author(s): John P. Lloyd and Clyde E. Kesler

Publication: Journal Proceedings

Volume: 67

Issue: 8

Appears on pages(s): 636-641

Keywords: anchorage (structural) ; bond (concrete to reinforcement) ; concrete slabs; cracking (fracturing) ; deformed reinforcement; one-way slabs; reinforced concrete; reinforcing steels; research.

Date: 8/1/1970

Abstract:
Forty-eight slabs were tested to determine the lice and anchorage requirements of deformed re and deformed wire fabric. The behavior of the slabs during the tests are described. Simple conservative design equations, taking into consideration the bond, weld and concrete strengths, are developed for computing the splice and anchorage lengths.