Title: Bond and Development of Steel Reinforcement in High-Strength Concrete-An Overview

Author(s): S.L. McCabe

Publication: Special Publication

Volume: 176

Issue:

Appears on pages(s): 1-22

Keywords: Bonding; cyclic loading; high-strength concrete; reinforced concrete

Date: 10/1/1998

Abstract:
Considerations regarding bond and development of reinforcement in high strength concrete (HSC) are presented from a North American perspective. The information contained in this paper is a compilation of information from various sources and represents a survey of the basis for North American approaches to bond of normal and high strength concrete under monotonic and cyclic loading. The paper was presented in part at the Second US-Japan-New Zealand-Canada Multilateral Meeting on the performance of HSC held in Honolulu November 29-December 1,1994.