Title: 362.1R-97: Guide for the Design of Durable Parking Structures (Reapproved 2002)
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 40
Keywords: Parking Structures
Date: 5/8/1997
Abstract:
Note: A newer version of this document exists. This document was replaced by 362.1R-12.
This guide is a summary of practical information regarding design of parking structures for durability. It also includes information about design issues related to parking structure construction and maintenance. The guide is intended for use in establishing criteria for the design and construction of concrete parking structures. It is written to specifically address aspects of parking structures that are different from those of other buildings or structures.