Title: Research on building Sandwich bearing panels carry out in the Laboratory of structuers in the ETS of ICC y P de Santander

Author(s): Arenas de Pablo, J. J.; Villegas Cabredo, L. M.; Gutierrez Martín, G.; Pedraja Fuentes, J.

Publication: ACHE

Volume: 36

Issue: 154

Appears on pages(s): 149 -