Title: Non-lineal analysis of prestressed concrete structures

Author(s): Murcia Vela, J.

Publication: ACHE

Volume: 37

Issue: 159

Appears on pages(s): 95 -

Keywords:

Date: 1/3/1986

Abstract:


ACI International Partner, ACHE Spain, International Partner Access.