Comparison of Eurocode 2, Model Code 90 and ACI 318-00 witregard to shear and punching provisions for footingsh

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparison of Eurocode 2, Model Code 90 and ACI 318-00 witregard to shear and punching provisions for footingsh

Author(s): Calavera Ruiz, J.

Publication: ACHE

Volume: 54

Issue: 230

Appears on pages(s): 81 - 84

Keywords:

DOI:

Date: 1/8/2003

Abstract:
Code ACI 318, MODEL CODE 90 and Eurocode EC-2 present important differences with regard to the shear strength and punching strength, this is especially shown when the steel ratio of rainforcement is low. The above mentioned is important especially in the case of footings. The author analyses the differences either in structural design or in cost for wall footings and isolated footings, in accordance with the three mentioned Codes.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »