Title: Influence of Relative Mechanical Strengths between New and Old Cement Mortars on the Crack Propagation of Recycled Aggregate Concrete

Author(s): Wengui Li, Zhihui Sun, Zhiyu Luo, Surendra P. Shah

Publication: JCI

Volume: 15

Issue: 3

Appears on pages(s): 110 - 125