Title: Evaluation of Shrinkage Induced Cracking in Concrete with Impact of Internal Curing and Water to Cement Ratio

Author(s): Jun Zhang, Yudong Han, Jiajia Zhang

Publication: JCI

Volume: 14

Issue: 7

Appears on pages(s): 324 - 334

Keywords:

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access.