Title: Evaluation of Alkalinity of Pore Solution Based on the Phase Composition of Cement Hydrates with Supplementary Cementitious Materials and its Relation to Suppressing ASR Expansion

Author(s): Yuichiro Kawabata, Kazuo Yamada

Publication: JCI

Volume: 13

Issue: 11

Appears on pages(s): 538 - 553

Keywords:

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access.