Title: Application of Sacrificial Point Anode for Prevention of Steel Corrosion in Cracked Concrete

Author(s): Muhammad Akbar Caronge, Hidenori Hamada, Rita Irmawaty, Yasutaka Sagawa, Daisuke Yamamoto

Publication: JCI

Volume: 13

Issue: 10

Appears on pages(s): 479 - 488

Keywords:

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access.