Title: Fundamental Study on Properties of Small Particle Size Porous Concrete

Author(s): Shigemitsu Hatanaka, Naoki Mishima, Akihiro Maegawa, Eisuke Sakamoto

Publication: JCI

Volume: 12

Issue: 1

Appears on pages(s): 24 - 33

Keywords:

Date: 1/1/2014

Abstract:


Japan Concrete Institute, International Partner Access.