Title: Change of the Coefficient of Thermal Expansion of Mortar Due to Damage by Freeze Thaw Cycles

Author(s): Evdon Sicat, Fuyuan Gong, Dawei Zhang, Tamon Ueda

Publication: JCI

Volume: 11

Issue: 12

Appears on pages(s): 333 - 346

Keywords:

Date: 1/1/2013

Abstract:


Japan Concrete Institute, International Partner Access.