Title: Fixed-Angle Smeared-Truss Approach with Direct Tension Force Transfer Model for Torsional Behavior of Steel Fiber-Reinforced Concrete Members

Author(s): Hyunjin Ju, Deuck Hang Lee, Jin-Ha Hwang, Kang Su Kim, Young-Hun Oh

Publication: JCI

Volume: 11

Issue: 9

Appears on pages(s): 215 - 229

Keywords:

Date: 1/1/2013

Abstract:


Japan Concrete Institute, International Partner Access.

View Resource »