Title: Mechanical, Electrical and Microstructural Properties of Cement-Based Materials in Conditions of Stray Current Flow

Author(s): Agus Susanto, Dessi A. Koleva, Oguzhan Copuroglu, Kees van Beek, Klaas van Breugel