Title: Ground Penetrating Radar: an Application to Estimate Volumetric Water Content and Reinforced Bar Diameter in Concrete Structures

Author(s): Giovanni Leucci

Publication: JCI

Volume: 10

Issue: 12

Appears on pages(s): 411 - 422

Keywords:

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access.