Title: Numerical Simulation on Shear Capacity and Post-Peak Ductility of Reinforced High-Strength Concrete Coupled with Autogenous Shrinkage

Author(s): Esayas Gebreyouhannes, Koichi Maekawa

Publication: JCI

Volume: 9

Issue: 1

Appears on pages(s): 73 - 88