Title: Inelastic Performance of High-Strength Concrete Bridge Columns under Earthquake Loads

Author(s): DaiJeong Seong, TaeHoon Kim, MyungSeok Oh, HyunMock Shin

Publication: JCI

Volume: 9

Issue: 2

Appears on pages(s): 205 - 220

Keywords:

Date: 1/1/2011

Abstract:


Japan Concrete Institute, International Partner Access.