Title: Effect of Tensile Loading on Chloride Penetration of Concrete Mixed with Granulated Blast Furnace Slag

Author(s): Dong Hun Kim, Kazunori Shimura, Takashi Horiguchi

Publication: JCI

Volume: 8

Issue: 1

Appears on pages(s): 27 - 34

Keywords:

Date: 1/1/2010

Abstract:


Japan Concrete Institute, International Partner Access.