Title: An Advanced Transient Concrete Model for the Determination of Restraint in Concrete Structures Subjected to Fire

Author(s): Ulrich Schneider, Martin Schneider

Publication: JCI

Volume: 7

Issue: 3

Appears on pages(s): 403 - 413

Keywords:

Date: 1/1/2009

Abstract:


Japan Concrete Institute, International Partner Access.

View Resource »