Title: Characterization for Long-Aged Hardened Cement Collected from Old Structures by Modern Technique for Chemical Analysis

Author(s): Daisuke Sawaki, Etsuo Sakai

Publication: JCI

Volume: 5

Issue: 3

Appears on pages(s): 325 - 332

Keywords:

Date: 1/1/2007

Abstract: