Title: Moisture Related Flooring Failure: The Causes and the Problems that Result

Author(s): Ryan A. Henkensiefken

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

Date: 3/23/2014

Abstract:
Due to several changes in the construction market, including EPA regulation changes to the allowable VOC content in adhesives and the rise of fast-track construction projects, moisture-related flooring failures have become more prevalent in concrete slab construction. In response, contractors have been seeking ways to combat these problems without impacting construction schedules.