In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Email Support
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: Early-Age Repair Material Properties
Author(s): Fred R. Goodwin
Publication: Web Session
Volume: Goodwin.pdf
Issue:
Appears on pages(s):
Keywords: early-age repair properties
Date: 4/15/2013
Abstract:The success and durability of many concrete repair projects depend on the early-age bond, strength development, modulus development, and dimensional stability of repair binders. Common repair methods that use these materials include concrete patching, overlays, and sprayed concrete. This session will focus on the early-age properties of new and innovative repair binders as determined by laboratory evaluation, field tests, and experience. New test methods for early-age properties of repair material will also be discussed.